SCOURING
(if needed)
Soap flake 2gram/liter
Soft Water
Heat up to 60°C, and keep 30min.
   
NYLON DYEING
(WOOL DYEING)
Selected Acid Dyes
1.0gram/liter Ammonium acetate
Soft Water Heat up to 90°C-95°C
Remain at chosen temperature for 30-45min.
   
RAYON DYEING Selected Direct Dyes
10 gram/liter Sodium Sulfate
Soft Water
Heat up to 90°C, and keep 30min.
 
IMPORTANT
Resistance durability would be declined if the yarn is elongated during weaving or knitting.
Re-dyeing not applicable
Please avoid all possible procedures in acidic and alkaline environments
The above data are obtained from our laboratory tests and are only indicative.
All customers are recommended to make their own laboratory tests in order to find the best possible conditions of protecting Metallic Yarn even sacrificing the fastness of finished fabrics to some extent.
 